Line 374: Line 374:
     * TLDR: 200C is a good starting point      * TLDR: 200C is a good starting point 
   - Cook until done   - Cook until done
 +    * TLDR: check every 15 minutes at 200C
     * Time varies greatly with temperature, epoxy type, and thickness     * Time varies greatly with temperature, epoxy type, and thickness
     * Solution opaque => difficult to monitor. You might need to pour to another container to check     * Solution opaque => difficult to monitor. You might need to pour to another container to check
Line 445: Line 446:
 ====== References ====== ====== References ======
   * http://zeptobars.ru/en/read/how-to-open-microchip-asic-what-inside   * http://zeptobars.ru/en/read/how-to-open-microchip-asic-what-inside
-  * CDCA: http://www.ecpe.org/fileadmin/_recycler_/07_Kerisit_Tools_Dedicated_to_Chip_Access.pdf+  * CDCA: 403 errors (as of Nov 2023), archived in Wayback Machine: http://web.archive.org/web/20180106035620/http://www.ecpe.org/fileadmin/_recycler_/07_Kerisit_Tools_Dedicated_to_Chip_Access.pdf 
 +    * Original URL: http://www.ecpe.org/fileadmin/_recycler_/07_Kerisit_Tools_Dedicated_to_Chip_Access.pdf
  
 
decap/epoxy_acid.txt · Last modified: 2023/11/18 11:49 by philpem
 
Except where otherwise noted, content on this wiki is licensed under the following license: CC Attribution 4.0 International
Recent changes RSS feed Donate Powered by PHP Valid XHTML 1.0 Valid CSS Driven by DokuWiki