40W CO2 laser can melt package, but it didn't evaporate. Also rest of package get severe thermal shock and cracked here and there | 40W CO2 laser can melt package, but it didn't evaporate. Also rest of package get severe thermal shock and cracked here and there | ||
- | {{: | + | {{: |
- | {{: | + | {{: |
Window was easily melted, but had a tendency to slice through the bond wires below | Window was easily melted, but had a tendency to slice through the bond wires below |